- E BK-92

Nickle Alloy Welding Electrode E BK 92

Nickle Based Welding Electrode E BK 92 For DC+ SMAW stock electrode. The reaction of titanium with carbon maintains a low level of free carbon and enables the filler metal to be used with Nickel 201. The weld metal has good corrosion resistance, particularly in alkali’s.

Applications

BK 92 is developed for welding and cladding Nickel 200 and Ni

1736: EL-NiTi3

ckel 201. This alloy is also suited for surfacing of steel. Dissimilar welding applications of filler metal NiTi 3 include joining Nickel 200 and 201 to stainless steels, copper-nickel alloys, and Monel alloys. It is also used for joining Monel alloys and coppernickel alloys to carbon steels, and for joining copper-nickel alloys to Inconel en Incoloy alloys.  

Classification

AWS

A 5.11: E Ni-1 F-No. 41

EN ISO 

14172: E Ni 2061 FM6

DIN

1736: EL-NiTi3

DIN: W.Nr  2.4156

Typical Weld Metal Analysis %

C Cu Fe Ti S P Mn Ni Si Al
0.10% 0.25% 1.9% 1.0-4.0% 0.02% 0.03% 0.75% 92% 1.25% 1.0%

Mechanical Properties (As Welded)

RP0,2 (N/mm2)
Rm (N/mm2)
A  (%)
          Impact Energy
 +20°C                         -196°C

414 MPa (60.0 PSi)
640 MPa (93 ksi)
>20%
>120                               >210

General Information

Welding process 

Covered Electrode (SMAW)

Alloy Type

Nickle Base 

Re-drying Temperature

300°C/2hours

Beads 

Use stringer beads (do not weave).


Cleaning

Remove all cracks and fatigued metal by grinding

Welding Parameters

Diameter & Length (mm)
Current (A)
2.5x300
70~80
3.2x300
90~120
4.0x350
120~150

 