- E-BK 309 MoL-16

Stainless Steel Welding Electrode E BK 309MoL-16

E 309MoL-16  This molybdenum-bearing stainless steel alloy, is especially suitable for joining all difficult to weld steels to themselves or to stainless steel, or for joining dissimilar stainless steels. The addition of Molybdenum provides higher corrosion resistance, higher strength, and creep resistance at elevated temperatures. When welding low and unalloyed steels, a weld good with high corrosion resistance is already obtained in the first layer. The deposited metal is resistant to hot cracking and is practically spatter and porosity free. Slag release is excellent, and weld pool control is easy to obtain. The welded deposit is heat resistant up to 1.050°C. (1.922°F).

Applications

joining of dissimilar steels. Welding of plated steels. For saltwater and pit type corrosive applications. Welding of CrNiMo stainless steels. Chemical, petrochemical, and food industry applications. Underlayer for stainless steel coatings. Do not use on applications that are continuously submitted to temperatures between 600 and 900°C.

Designed with low carbon levels to help eliminate carbide precipitation in high temperature service 

Classification

AWS

AWS A5.4 : E309MoL-16

EN ISO 

------

DIN

-------


Typical Weld Metal Analysis %

C Mn Mo Cr Ni Si P S F
0.03% 0.6-1.2% 2-2.5% 22.5-23.5 9% 1% <0.025% <0.025% Bal.

Mechanical Properties (As Welded)

RP0,2 (N/mm2)
Rm (N/mm2)
A  
(%)

Impact Energy
 Charpy V notch (ISO-V)

350 >650
>30
           60 J (20°C)

General Information

Welding process 

Covered Electrode (SMAW)

Alloy Type

High alloyed steel

Re-drying Temperature

300°C/2hours

Welding   Position  

All, except vertical down.


Cleaning

Remove all cracks and fatigued metal by grinding. 

Welding parameters

Diameter & Length (mm)
Current (A)
2.5x300
70~80
3.2x300
90~120
4.0x350
120~150

Instruction:

Weld with low heat input.

Electrode to be held perpendicular to the workpiece.

Preheating is necessary when joining high carbon steel ( 150 -250°C).

keep a short arc: Allow the welded area to cool down slowly.

For welding stainless steel, the coating must not be damaged and it is recommended to return over the starting point of the bead. 

 